Use of reference:
1. With OX280 every tons of latex about 25-37.5 KG powder.
2. Use first cold or warm water will starch move into powder milk, the powder: water 1:1-1:1. 5 (depending on the latex concentration request)
3. In latex polymerization are about to finish, material temperature 80 to 90 degrees centigrade join. When feeding should slow to join, avoid temperature urgent drop.
4. Add to finish, maintain milk powder in the former 80 to 90 degrees Celsius heat preservation continue reaction, to temperature reduced to ordinary discharging temperature can be the material.